Slump Test for Concrete | Procedure and Interpretation of Results


SPONSORED

Slump Test for Concrete | Procedure and Interpretation of Results


Slump Test for Concrete | Procedure and Interpretation of Results

The concrete slump test measures the consistency of fresh concrete before it sets. It is performed to check the workability of freshly made concrete, and therefore the ease with which concrete flows. It can also be used as an indicator of an improperly mixed batch. The test is popular due to the simplicity of apparatus used and simple procedure. The slump test is used to ensure uniformity for different loads of concrete under field conditions.

Procedure for Slump Test for Concrete

The test is carried out using a metal mould in the shape of a conical frustum known as a slump cone or Abrams cone, that is open at both ends and has attached handles.

The tool typically has an internal diameter of 100 millimetres (3.9 in) at the top and of 200 millimetres (7.9 in) at the bottom with a height of 305 millimetres (12.0 in).

The cone is placed on a hard non-absorbent surface. This cone is filled with fresh concrete in three stages.

Each time, each layer is tamped 25 times with a 2 ft (600 mm)-long bullet-nosed metal rod measuring (16 mm) in diameter.

At the end of the third stage, the concrete is struck off flush with the top of the mould. The mould is carefully lifted vertically upwards, so as not to disturb the concrete cone.

The concrete then slumps (subsides). The slump of the concrete is measured by measuring the distance from the top of the slumped concrete to the level of the top of the slump cone.


Result of Slump Test

The slumped concrete takes various shapes, and according to the profile of slumped concrete, the slump is termed as true slump, shear slump or collapse slump. If a shear or collapse slump is achieved, a fresh sample should be taken and the test repeated. A collapse slump is an indication that the mix is too wet.

types of slump

Only a true slump is of any use in the test. A collapse slump will generally mean that the mix is too wet or that it is a high workability mix, for which the slump test is not appropriate. Very dry mixes having slump 0 – 25 mm are typically used in road making, low workability mixes having slump 10 – 40 mm are typically used for foundations with light reinforcement.

Medium workability mixes with slump 50 – 90 mm, are typically used for normal reinforced concrete placed with vibration, high workability concrete with slump higher than 100 mm is typically used where reinforcing has tight spacing, and/or the concrete has to flow a great distance.

Limitations of the Slump Test

The slump test is suitable for slumps of medium to high workabiity, slump in the range of 5 – 260 mm, the test fails to determine the difference in workability in stiff mixes which have zero slump, or for wet mixes that give a collapse slump. It is limited to concrete formed of aggregates of less than 38 mm (1.5 inch).